Zostałaś(eś) przekierowany do lokalnej wersji strony

AB-205

Thermostability of PVC and other chlorine-containing polymers


Summary

This Application Bulletin describes the determination of the thermostability of PVC in accordance with ISO 182 Part 3 using the dehydrochlorination method with the 895 Professional PVC Thermomat. The instrument permits fully automatic determination of the stability time. The test is suitable for monitoring the manufacture and processing of PVC products manufactured in the injection molding process, for their final clearance, characterization and for the comparison of PVC products and for testing the effectiveness of heat stabilizers.

 

 